DaveinOlyWA
Well-known member
Marktm said:Similar data report for my 2021 SV Plus. Appears faster (time & miles) degradation than Gary's. It has been summer here in Houston, TX, but it is garage kept, very seldom left in sun, battery temps in the low 80's and gently charged (not one QC):
Batter log 8.20.21.jpg
On the flipside (with another adjustment before the two year mark) despite having much warmer than normal weather, I am still nowhere near the heat onslaught either of you have seen and adjusting for mileage and time, I will likely be just about where you two are as well.
I am approaching 8% loss (for 2nd time) on SOH but interesting enough, it looks like I will also be around 7½% loss on kwh available and GID.